The invention relates to a method for hybrid gas carbonitriding of alloy steels in fluidized-bed furnaces, particularly carbon and alloy steels with a carbon content of up to 0.25% and alloying additions of Cr, Ni, Mn, Mo and Ti, intended to increase the hardenability of the steel while preserving the ductility of the core. The method involves carburizing steel or cast-iron parts at a temperature of 900 °C in an endothermic atmosphere generated by the incomplete combustion of propane or natural gas in the presence of a nickel (Ni) catalyst, followed by nitriding, which consists of saturating the parts with nitrogen at an elevated temperature in a nitrogen-containing atmosphere, with ammonia as the nitrogen carrier (2NH3 -> 6H+2N), and is characterized in that, in the first stage, the structure of the steel or cast-iron parts is stabilized and opened up by nitriding at a temperature of 900 °C to 950 °C for 5 minutes to 15 minutes in a nitrogen-containing atmosphere; in the second stage, the steel or cast-iron parts are carburized at a temperature above the Ac3 austenitic transformation temperature, in the range of 900 °C to 950 °C, for 20 minutes to 40 minutes in an endothermic atmosphere generated by the incomplete combustion of propane or natural gas in the presence of a nickel (Ni) catalyst; and in the third stage, the steel or cast-iron parts are hardened by carbonitriding at a temperature of 900 °C to 950 °C for 15 minutes to 30 minutes in a nitrogen-containing endothermic atmosphere, after which the steel or cast-iron parts, at a temperature of 900 °C to 950 °C, are quenched in oil at a temperature of 40 °C to 90 °C.